news
Home > News > Industry news > PVC Profile Production Methord

News

PVC Profile Production Methord

  • Author:Laura
  • Source:Baidu
  • Release on :2017-02-22

PVC Profile Production Methord

 

Storage


 

PVC Profiles in the transport process to avoid contact with the hard, rough and sharp objects friction, in the storage process to avoid high temperature, sun, rain, oil, corrosive chemicals, dust and other damage. Shields in the outdoor storage, there must be shelter protection measures, non-white profiles should be stored away from light.

 

Cutting

Cutting Speed:60-70m/sec

To ensure proper feed speed; blunt serrated or too fast feed speed can lead to incision defect.

Accurate adjustment of the blade angle is 45 degrees, the maximum angle error of 0.5 degrees.

Strictly in accordance with the given length limit, the length of the error does not exceed 0.5mm.

The cut section should be placed under the incision, and 48 hours to complete the welding, so as not to cause too long storage surface pollution, affecting the quality of welding .

 

Drilling and milling

 

The feed rate and the cutting speed of the borehole are reduced as the drilling depth increases;

Drill hole diameter greater than 20mm hole should use double slot drill, drill diameter greater than 40mm hole should be used to gradually change the drill bit .

 

Welding

Welding parameters, meet the following requirements:

Welding plate temperature: 245-250 degrees;

Warm-up time:>30s;

Pressing Time:>30s;

Welding pressure:0.2-0.3MP;

The weld can not get yellow;

Welding angle to avoid sharp cooling after finishing welding, severe impact, clear angle or around the welding seam milling cutting process should be completed at least 1 minutes after welding.

 

Clearance angle

Welding cooling can not be added in any way;

Clear the best angle in the welding completed: 1 minute -30 minutes to ensure the welding strength and access to high-quality angle seam cleaning effect;

Welding angle on both sides of the plane of the decorative slot width is 3mm, the concentration is not greater than 0.3mm ;

The cutting depth is too large or too blunt to clean up because of the tool in percussion will lead to reduced increasing the strength of fillet weld ;

Angle (especially the sealing strip embedded groove) cut too deep or too big to reduce the effect of welding angle, and water tightness .


Setting-in

Any tape can not be too much tension, and to ensure that the plastic length of about 2% longer than the embedded slot. Flat window frame fan seal is a week around a tape, the dock should be on the side of the middle, do not dock at the corner, not to cut into several paragraphs. Strip in the corner to be flat.

Press the sealing surface of the glass should be at the corner of the 45 degree cut butt, to ensure that the length of the rubber strip and the cutting angle of the close together.

Select the appropriate type seal according to the glass thickness.

Sealing strip must be completely into the groove to ensure the sealing effect and the normal installation of glass.

There are not many connections in the same slot.